Penetration Grades

Tests Title
Method
Unit
Guarantee Range
Unit
Guarantee Rangeas
Penetration @25°C
ASTM D70
0.1mm
60-70
0.1mm
85-100
Density @25°C
ASTM D5
g/cm³
1.01-1.06
g/cm³
1.01-1.05
Ductility @25°C
ASTM D113
cm
100 min
cm
100 min
Flash Point
ASTM D92
°C
230 min
°C
230 min
Sotfening Point
ASTM D36
°C
46 min
°C
42 min
Spot Test
AASHTO T102
---
Negetive
---
Negetive
Solubility in TCE
ASTM D2042
%wt
99 min
%wt
99 min
Loss On Heating
ASTM D6
%wt
0.2 max
%wt
0.5 max
Drop in Penetration After Heating
ASTM D5
%
20 max
%
20 max
Cheng mass After (TFOT)
ASTM D1754
%
0.8 max
%
1 max
Retained Penetration After (TFOT)
ASTM D5
%
52 min
%
47 min




cm
75 min

The most production type of bitumen in the world is petroleum bitumen, which is obtained from crude oil distillation, and they are mostly classified based on penetration, viscosity and performance grade.
About penetration, 60-70, 85-100 are the most popular and used kinds, so the main market shares are mostly Pacific Asia, and Africa. India.
About viscosity, VG 40, VG 30 are the most used and common kinds in India.

Available way of transporting:
• DRUM: 150, 180 ,200 kg
• JUMBO: 1000 kg , 1300 kg , 300 kg
• BULK

Viscosity Grades

Product Specification Viscosity Grad Bitumen
VG 40
VG 30
Test Method
Absolute Viscosity at 60°C, Poises (min)
3200
2400
ASTM D-2171
Kinematic Viscosity at 135°C, cSt (min)
400
350
ASTM D-2170
Flash Point (Cleve Land Open Cup) °C (min
220
220
ASTM D-92
Solubility in tricholoroethylene, % (min)
99
99
ASTM D-2040
Softening Point (R&B), °C
50
47
ASTM D-36
Penetration @ 25°C(100 g, 5 sec.),0.1 mm
40 - 60
50 - 70
ASTM D-5
Specific Gravity @ 27/27°C (min)

0.99
0.99
ASTM D-70

VG 40
VG 30
Test method
Absolute Viscosity at 60°C, Poises

Min.3200
Min.2400
IS 1206 (Part 2)
Kinematic Viscosity at 135°C, cSt
Min.400
Min.350
IS 1206 (Part 3)
Flash Point (Cleveland Open Cup) °C
Min.220
Min.220
IS 1206
Solubility in trichloroethylene %
Min.99
Min.99
IS 1206
Softening Point (R&B), °C
Min.50
Min.47
IS 1205
Penetration @ 25°C(100 g, 5 sec.),0.1 mm
40-60
50-70
IS 1203
I) Viscosity ratio at 60°C

Max .4.0
Max.4.0
IS 1206 (Part 2)
ii) Ductility at 25°C, cm, after thin film oven test
Min.25
Min.40
IS 1208
Specific Gravity @ 27/27 °C
Min.0.99
Min.0.99
IS 1202

Others

SPECIFICATION
TEST METHOD
UNIT
10/20
40/50
60/70
80/100
Specific Gravity @25°C
ASTM D-70
-
1.01-1.06
1.01-1.06
1.01-1.06
1.06
Pentration @25°C, 100gr, 5 Sec
ASTMD-5
0.1 mm
10-20
40-50
60-70
80-100
Softening Point, Ring & Ball, °C
ASTMD-36
°C
52-60
52-60
49-56
45-52
Ductility @25°C , min
ASTMD-113
cm
100.0
100.0
100.0
100.0
Ductility @10°C , min
ASTMD-113
cm
-
-
-
-
Loss on Heating , max
ASTMD-6
%wt
0.8
0.8
0.8
1
Drop in Penetrstion after heating , max
ASTM D-5 & D-6
%wt
20.0
20.0
20.0
20.0
Flash Point Cleveland open-cup , min
ASTMD-92
°C
230
230
230
230
Solubility in CS, min
ASTMD-4
%wt
99.5
99.5
99.5
99.5
Organic Matter Insoluble in CS, max
ASTMD-4
%wt
0.5
0.5
0.5
0.5
Spot test
*A.AS.H.T.O.102
-
Negetive
Negetive
Negetive
Negetive

 

Our main suppliers :

  • Pasargad oil
  • Jey oil
  • Horomozan
  • Psargad Energy Development                                                           

We offer Flexible and Convenient delivery options for any destination.

whether you prefer bulk, flexibag/tanks, drum.
we have it all for you. just let us know your preference and requirements.